Black and white incised stoneware mug

$40.00

Black and white incised stoneware mug

SKU: AJ24089 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24089
Run/Test Number: P6731
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, bisque fired, dip glazed

Firing ScheduleC10RPL
TemperatureCone 10R
Glaze InsideGR10-C
Glaze OutsideGR10-C
EngobeL3954N
Clay BodyH550
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 100 mm (3.9 in)
Depth at rim (including handle) – 133 mm (5.2 in)
Height – 110 mm (4.3 in)
Weight – 363 grams (12.8 oz)

Registration Page: https://digitalfire.com/potterytony/2430

Weight 363 g
Dimensions 133.00 × 100.00 × 110.00 mm