Red and black porcelain mug

$50.00

Red and black porcelain mug

SKU: AJ24304 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24304
Run/Test Number: P6886
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing SchedulePLC6DS
TemperatureCone 6
Glaze InsideG2926BL
Glaze OutsideG2934Y Red
Clay BodyM370
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 100 mm (3.9 in)
Depth at rim (including handle) – 135 mm (5.3 in)
Height – 130 mm (5.1 in)
Weight – 429 grams (15.1 oz)

Registration Page: https://digitalfire.com/potterytony/2436

Weight 429 g
Dimensions 135.00 × 100.00 × 130.00 mm