Red Polar Ice porcelain mug

$40.00

Red Polar Ice porcelain mug

SKU: AJ24086 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24086
Run/Test Number: P6803
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside

Firing SchedulePLC6DS
TemperatureCone 6
Glaze InsideG2926B
Glaze OutsideG2934Y Red
Clay BodyPolar Ice
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 89 mm (3.5 in)
Depth at rim (including handle) – 121 mm (4.8 in)
Height – 104 mm (4.1 in)
Weight – 312 grams (11.0 oz)

Registration Page: https://digitalfire.com/potterytony/2424

Weight 312 g
Dimensions 121.00 × 89.00 × 104.00 mm