Honey glazed MNP/porcelain mug

$30.00

Blend of MNP and M370

SKU: AJ24368 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24368
Run/Test Number: L4491
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside. I process raw clay lumps manually by slaking, slurry-up, sieving and dewatering on a plaster table.
Description: Blend of MNP and M370

Firing ScheduleC6DHSC
TemperatureCone 6
Glaze InsideG2926B white
Glaze OutsideGA6-B
Clay BodyMNP M370 mix
Foot Style – Unglazed flat
Width at rim (perpendicular to handle) – 94 mm (3.7 in)
Depth at rim (including handle) – 123 mm (4.8 in)
Height – 116 mm (4.6 in)
Weight – 354 grams (12.5 oz)

Registration Page: https://digitalfire.com/potterytony/2554

Weight 354 g
Dimensions 123.00 × 94.00 × 116.00 mm