White glossy glazed reduction fired mug

$50.00

White glossy glazed reduction fired mug

SKU: AJ24423 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24423
Run/Test Number: L4453E
Technique: Thrown, incised, dip-glazed

Firing ScheduleC10RPL
TemperatureCone 10R
Glaze InsideGR10-A
Glaze OutsideGR10-A
Clay BodyH550
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 100 mm (3.9 in)
Depth at rim (including handle) – 128 mm (5.0 in)
Height – 117 mm (4.6 in)
Weight – 395 grams (13.9 oz)

Registration Page: https://digitalfire.com/potterytony/2556

Weight 395 g
Dimensions 128.00 × 100.00 × 117.00 mm