Floating-blue stoneware mug

$35.00

Floating-blue stoneware mug

SKU: AJ24318 Category:

For detailed information on my R&D and the mugs that are a product of it please go to https://tonyhansen.com/pottery.

Serial Number: AJ24318
Run/Test Number: P6904
Technique: Thrown, engobed inside and top outside at leather hard stage, incised, liner-glazed inside, dip-glazed outside

Firing SchedulePLC6DS
TemperatureCone 6
Glaze InsideG3914A
Glaze OutsideGA6-B
EngobeL3954B
Clay BodyM340
Foot Style – Fluted ring
Width at rim (perpendicular to handle) – 101 mm (4.0 in)
Depth at rim (including handle) – 132 mm (5.2 in)
Height – 115 mm (4.5 in)
Weight – 446 grams (15.7 oz)

Registration Page: https://digitalfire.com/potterytony/2463

Weight 446 g
Dimensions 132.00 × 101.00 × 115.00 mm